Maoming Optimal Heat Dissipation Copper Foil Processing
The air supply of general air conditioning has a large impact. For the stains caused by the dirty electrolyte, the filtering of electrolyte should be strengthened. After being transferred from the electrolytic cell, the copper foil must be washed with electrolyte, because the surface of the copper foil is attached with organic matter or other impurities. The water pressure of copper foil washing must have enough pressure and a certain amount of water.
Maoming Optimal Heat Dissipation Copper Foil Processing
Electrolytic copper foil is made by dissolving copper into copper sulfate solution, electrodepositing the copper sulfate electrolyte under the action of direct current in special electrolytic equipment to make the original foil, and then carrying out surface treatment, heat-resistant layer treatment, oxidation prevention treatment and other surface treatment processes on the original foil according to customer requirements.
Maoming Optimal Heat Dissipation Copper Foil Processing
Silane coupling agent treatment: after anti oxidation treatment, the surface is sprayed with silane, which can improve the oxidation resistance at room temperature on the one hand; On the other hand, in high temperature pressing plate, silane can better combine copper foil and resin substrate through coupling, and improve peel strength. Post treatment process - drying. In order to prevent the harm of residual moisture, it must be dried at not less than 100 ℃ later, and the drying temperature cannot be too high.
Maoming Optimal Heat Dissipation Copper Foil Processing
The calendered copper foil is made by repeated rolling annealing process of copper ingot based on the principle of plastic processing. Its internal structure is lamellar crystal structure, and the product has good ductility. At present, it is mainly used in the production of rigid circuit boards, while the rolled copper foil is mainly used in flexible and high-frequency circuit boards.
Maoming Optimal Heat Dissipation Copper Foil Processing
If the surface stain is caused by environmental problems, the cleaning and improvement of the air conditioning filter system should be strengthened, or the wind speed should be reduced, and the small hairs on the air conditioning filter bag must be completely removed. And the fibers and powders on the polymer materials must be completely removed, which are very easy to cause stains. The air supply pipeline is easy to use plastic material, which does not produce fiber and is easy to clean with water, acid and alkali.
Maoming Optimal Heat Dissipation Copper Foil Processing
Galvanizing barrier layer: After the rough surface is galvanized, a barrier layer is formed to improve the oxidation resistance of the copper foil in natural air. After galvanizing, the appearance will look gray. After a period of storage, the gray will turn into copper yellow. The more zinc is plated, the more yellow the copper foil will be.