Shanwei Optimum Electrolytic Copper Foil Price
At the same time of thinning, it is also necessary to improve the tensile strength, elongation and other indicators, otherwise it is easy to cause copper foil fracture, affecting the safety of the battery. Therefore, it is the general trend that the future use will be more light and meet the above indicators.
Shanwei Optimum Electrolytic Copper Foil Price
Small dirt, small exclamation mark. During the production of raw foil, the hair side is upward, and the dirt in liquid and air all fall on the hair side, which is printed on the smooth side after rolling. The reason is that the stains on the cathode roll are not dried. The surface temperature of the cathode roll is only 50 degrees, and the air temperature in the workshop is generally about 25 degrees. The surface hairiness is very good. The dirt itself has water, and the drying time is only 2-3 minutes. Therefore, the dirt on the copper foil cannot be completely dried.
Shanwei Optimum Electrolytic Copper Foil Price
The production of extremely thin copper foil has high barriers, and the products produced still need to meet many requirements of downstream lithium ion battery manufacturers. For investors, they should not only focus on the single index of thickness, not all manufacturers produce 6 μ M Copper foil is consistent, and the thinner the better.
Shanwei Optimum Electrolytic Copper Foil Price
During the production of copper foil, tiny foreign matters are adhered on the surface to form spots with different colors from the surface, which are called stains. Judgment method: use macroscopic inspection to judge whether it is a waste product, a secondary product or a finished product according to the number and area of stains and the impact on product quality.
Shanwei Optimum Electrolytic Copper Foil Price
Copper foil can be divided into many kinds according to different classifications. According to the thickness, it can be divided into: thickness (more than 70 μ m) Regular thickness copper foil (more than 18 μ M but less than 70 μ m) Thin copper foil (more than 12 μ M but less than 18 μ m) Ultra thin copper foil (less than 12 μ m) Etc.
Shanwei Optimum Electrolytic Copper Foil Price
Copper foil is a key conductive material in lithium ion batteries and printed circuit boards. It is a kind of negative electrolytic material, a thin, continuous metal foil deposited on the substrate of circuit board.