Taizhou Optimal Anti static Copper Foil Processing
Electronic circuit copper foil plays an important role in conducting electricity and heat in printed circuit board (PCB), and is known as the neural network on PCB. At present, copper foil for electronic circuits (PCB copper foil) is divided into two categories, namely conventional copper foil and high-performance copper foil.
Taizhou Optimal Anti static Copper Foil Processing
Copper foil can be divided into many kinds according to different classifications. According to the thickness, it can be divided into: thickness (more than 70 μ m) Regular thickness copper foil (more than 18 μ M but less than 70 μ m) Thin copper foil (more than 12 μ M but less than 18 μ m) Ultra thin copper foil (less than 12 μ m) Etc.
Taizhou Optimal Anti static Copper Foil Processing
The calendered copper foil is made by repeated rolling annealing process of copper ingot based on the principle of plastic processing. Its internal structure is lamellar crystal structure, and the product has good ductility. At present, it is mainly used in the production of rigid circuit boards, while the rolled copper foil is mainly used in flexible and high-frequency circuit boards.
Taizhou Optimal Anti static Copper Foil Processing
The production process of electrolytic copper foil is simple. There are three main processes: solution raw foil, surface treatment and product slitting. The production process seems simple, but it is a production process that integrates electronics, machinery and electrochemistry, and is particularly strict with the production environment. Therefore, the industry does not have a set of standard and universal production equipment and technology, and each manufacturer shows its own ingenuity, which is also an important bottleneck affecting the improvement of domestic production capacity and quality.
Taizhou Optimal Anti static Copper Foil Processing
Small dirt, small exclamation mark. During the production of raw foil, the hair side is upward, and the dirt in liquid and air all fall on the hair side, which is printed on the smooth side after rolling. The reason is that the stains on the cathode roll are not dried. The surface temperature of the cathode roll is only 50 degrees, and the air temperature in the workshop is generally about 25 degrees. The surface hairiness is very good. The dirt itself has water, and the drying time is only 2-3 minutes. Therefore, the dirt on the copper foil cannot be completely dried.